Lipstick moulds are split metal moulds in which molten lipstick mass is cast into sticks. These are made of brass and come with 4 holes or 6 holes. Once the mass has set, the two halves are opened and the finished sticks are lifted out for fitting into cases.
Specifications
| Material | Brass |
| Cavities | 4 holes or 6 holes |
| Minimum order quantity | 10 units |
| Dispatch time | Usually 4–6 working days |
| Manufacturer | JLab (Jain Laboratory Instruments Pvt Ltd), Ambala, India |
Cosmetics Practicals with the Mould
Preparing a lipstick is a standard practical in pharmacy and cosmetics courses. Students first grind the colour into a little castor oil in a Porcelain Pestle and Mortar so that no specks remain. They melt the waxes and oils together in a beaker on a Water Bath Rectangular, stir in the coloured oil and pour the melt into the greased mould.
When the sticks have set, students scrape the surplus off the top with an SS Ointment Spatula and open the mould. Teachers often have groups cast two formulas side by side and compare the sticks for hardness, gloss and breakage.
Frequently Asked Questions
Why should the mould be greased before pouring?
A thin film of release agent, such as liquid paraffin, stops the set mass sticking to the brass. Without it, sticks tear or snap as the halves are opened. Wipe off any surplus so it does not mark the surface of the sticks.
What causes holes or air pockets in the cast sticks?
Air is beaten in by fast stirring, or trapped when the mass is poured too cool and thick. Stir gently, let the melt stand briefly so bubbles can rise, and pour in one steady stream held close to the mould.
Should the mould be warm or cold when I pour?
Warm it slightly first. A very cold mould sets the outside of the stick at once and can trap air or leave cold marks. After pouring, the filled mould can be chilled so the sticks shrink a little and come out cleanly.
Why do my sticks break when I take them out?
Usually the mass has not fully set, or the mould was not greased. Let it cool completely, scrape the top level and open the halves evenly. A formula with too little wax also gives soft, weak sticks.
Should I choose the 4-hole or the 6-hole mould?
Both are brass and work the same way. The 6-hole mould casts more sticks from one melt, which suits a class batch. The 4-hole mould suits small trial batches when students compare formulas.