PPR Welding Machine Manufacturer,Supplier and Exporter in India
Product Code : EL-PWI-8823
Jlab Export is a leading PPR Welding Machine Manufacturer,and suppliers in India
PPR water pipes are joined by socket fusion. The pipe end and the fitting socket are heated on the heating bushes, then pushed together so the plastic fuses into one piece. This machine takes pipe from 20 mm to 63 mm on its copper head. It has a temperature regulator and two heating switches, and it comes in a metal case with a pipe cutter, measuring tape, Allen key and holding stand.
Specifications
| Use | Welding plastic (PPR) pipe |
| Pipe size | 20–63 mm |
| Heating head | Copper |
| Temperature control | Regulator to set the welding temperature |
| Heating switches | Two |
| Accessories | Pipe cutter, measuring tape, Allen key, holding stand |
| Case | Metal carrying case |
| Minimum order quantity | 1 unit |
| Dispatch time | Usually 14–18 working days |
| Manufacturer | JLab (Jain Laboratory Instruments Pvt Ltd), Ambala, India |
PPR Jointing Practicals for Plumber Trainees
Trainees cut PPR pipe square with the pipe cutter from the case and mark the socket depth with the measuring tape. With the machine on its stand at welding temperature, they push the pipe and the fitting onto the bushes and hold them for the heating time. Then they join them in one straight push, without twisting, and leave the joint to cool.
A fuller exercise runs a short hot and cold PPR line to a pair of Basin Pillar Taps. The line is tested with a Pressure Testing Pump before the taps are opened. Teachers can cut a finished joint along its length to show the fused bead inside and out, next to a joint that was heated too little.
Frequently Asked Questions
What pipe sizes can it join?
It welds PPR pipe and fittings from 20 mm to 63 mm. For each size, a matching pair of heating bushes is fixed to the copper head, one for the pipe and one for the fitting socket.
What temperature should be set for PPR?
Set the temperature regulator to the welding temperature given by the pipe maker, and wait until the head has reached it before the first joint. Welding on a head that is still warming up gives weak joints.
How long should the pipe and fitting be heated?
Heating, joining and cooling times depend on the pipe size and wall thickness, and the pipe maker gives them in a chart. Larger pipe needs longer heating. Hold the joint still for a few seconds after pushing it together, then let it cool before moving it.
What causes a bad PPR joint?
The usual faults are a pipe end that is not square, a dirty or wet surface, and too little or too much heat. Twisting the pipe while pushing it in also spoils the joint. Too much heat or force throws up a large bead that narrows the bore.